SUS 304 Austenitic Stainless Steel, SAE 304, Werkstoff 1.4301, UNS S30400, DIN X 5CrNi18-10
Price:
R.F.Q.
Share Product:
Detail
Trade Name | Technical Delivery Condition | Annealed Hardness | C (%) | Si (%) | Mn (%) | Cr (%) | Ni (%) |
---|---|---|---|---|---|---|---|
SUS304 | Annealed | 187 HB | ≤ 0.08 | ≤ 1.00 | ≤ 2.00 | 18.00 – 20.00 | 8.50 - 10.50 |
Werkstoff | DIN standard | AISI | BS | JIS | SIS | UNI |
---|---|---|---|---|---|---|
1.4301 | X5CrNi18-10 | 304 | 304 | SUS 304 | 2332 | X5CrNi18-10 |
Type of steel and characteristics:
Austenitic chromium nickel steel. In the condition of supply, resistance to inter granular corrosion in the temperature range up to 300°C is good in sheet of up to 6 mm thickness and bar of up to 40 mm diameter.
These size ranges do not require any post-weld heat treatment The steel resists weathering, it possesses good resistance to the action of steam, water and acids as well as alkaline solutions. For optimum resistance, surface should be pick led.
Cold forming properties are good. The steel is capable of taking a mirror finish.
Applications:
For architectural purposes, household appliances, catering equipment, cutlery industry, medical equipment, automotive industry, sanitary equipment
Heat Treatment:
Hot Forging - 1200 - 900°C
Quenching Medium - 1000 - 1100°C
Structure as solution annealed: Austenite (+ small ferrite percentages)